MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® 2712 HDPE Injection Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Features: Good stiffness and impact resistance, minimal warpage, good top loading capability, high surface gloss.

Applications: Aerosol overcaps, food containers, frozen food containers, seedling trays, berry boxes.

Data provided by the manufacturer.

Key Words: High Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.951 g/ccASTM D792
Melt Flow 32 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow 30.5 cmNOVA Snake Flow Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ASTM D2240
Tensile Strength, Yield 23.0 MPaASTM D638
Elongation at Break 200 %ASTM D638
Flexural Modulus 1.00 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 120 °CASTM D1525
Brittleness Temperature <= -70.0 °CASTM D696
 
Processing PropertiesOriginal ValueComments
Melt Temperature 170 - 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding
Dow DMDA-8920 NT 7 High Density Polyethylene Resin
NOVA Chemicals Sclair® 2815 HDPE Injection Molding Resin
NOVA Chemicals Sclair® IG464-C Injection Molded HDPE Resin
Braskem ML3601U LLDPE Rotomolding Polyethylene

PEHN1Q / 35575

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.