MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo Plexiglas® HT121 Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Heat Resistant, Molded

Material Notes: Plexiglas® HT121 is a thermoplastic acrylic resin formulated for injection molding applications. It is characterized by its high heat resistance. Plexiglas® HT121 has excellent weatherability and optical properties allowing it to excel in applications requiring outdoor stability, high quality surface appearance and/or precision optics. It has excellent resistance to many chemicals including solutions of inorganic acids, alkalis and aliphatic hydrocarbons such as VM&P naphtha and heptane. Additionally, it is virtually unaffected by a wide range of commercial products including many beverages, foodstuffs, detergent solutions and cleaners.

Appearance: Clear/Transparent; Colors Available; Opaque; Translucent

Characteristics: High Clarity; High Scratch Resistance; Good Color Stability, Good Dimensional Stability; Low Shrinkage; Good Thermal Stability, Good UV Stability; High Heat Resistance; Good Weather Resistance

Applications: Automotive Applications; Lighting Diffusers

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Water Absorption 0.40 %24 Hour immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 in/inASTM D955
Melt Flow 2.6 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 99ASTM D785
Tensile Strength, Ultimate 10200 psiASTM D638
Elongation at Break 3.0 %ASTM D638
 3.0 %ASTM D638
Tensile Modulus 475000 psiASTM D638
Flexural Yield Strength <= 15200 psiASTM D790
Flexural Modulus 475000 psiASTM D790
Izod Impact, Notched 0.300 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.30 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 235 °FAnnealing cycle: 4hrs at 95°C; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 226 °FAnnealing cycle: 4hrs at 95°C; ASTM D648
Vicat Softening Point 240 °C
@Load 0.0000510 kg
50°C/hr; ASTM D1525
 246 °F
@Load 1.02 kg
50°C/hr; ASTM D1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49
@Wavelength 589.3 nm
ND; ASTM D542
Haze <= 1.0 %
@Thickness 3.17 mm
ASTM D1003
Transmission, Visible 92 %
@Thickness 3.17 mm
ASTM D1003
 
Descriptive Properties
ASTM ClassificationPMMA 014 1 V2ASTM D788

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Plexiglas® V825 Acrylic
Evonik ACRYMID® TT50 Acrylic Molding Compound
Chi Mei Acryrex® CM-205 PMMA
Trinseo Plexiglas® V826 Acrylic
Lotte Advanced Materials Infino® WP-1089 PC/ABS, Unreinforced

PARKG044b / 108347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.