MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Diamond DIAMALOY GLY 9020 Sheet Extrusion Grade
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Diamaloy GLY 9020 resin is a high-gloss, low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it can be easily coextruded. This product is supplied in various colors.

Applications: Typical applications include those requiring weatherability and high gloss such as body panels for tractors, recreational vehicles, etc. As with any product, use of Diamaloy GLY 9020 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Weatherable Polymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 7.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 38.0 MPachs 2.0 in/min; ASTM D638
Tensile Strength, Yield 56.0 MPachs 2.0 in/min; ASTM D638
Elongation at Break 15 %chs 2.0 in/min; ASTM D638
Elongation at Yield 3.0 %chs 2.0 in/min; ASTM D638
Flexural Strength 82.0 MPa
@Thickness 3.17 mm
chs 0.05 in/min; 2 in span; ASTM D790
Flexural Modulus 2749 MPa
@Thickness 3.17 mm
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 107 J/m
@Thickness 3.17 mm
ASTM D256
Instrumented Impact Total Energy 32.7 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 53.0 µin/in-°F
@Temperature -40.0 - 37.8 °C
ASTM E831
CTE, linear, Transverse to Flow 60.0 µin/in-°F
@Temperature -40.0 - 37.8 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C0.125";; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C0.125";; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond DIAMALOY GLY FXW749 Sheet Extrusion Grade, Sparkle/Pearlescence
A. Schulman Diamond DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer
A. Schulman Diamond DIAMALOY GLY 7010 Sheet Extrusion Grade
A. Schulman Diamond Centrex® 825 Sheet Extrusion Grade
A. Schulman Diamond Centrex® 821 ASA Weatherable Polymers Injection Molding Grade

PDIAM399 / 126490

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.