MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crucible Steel 440C Chromium Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Crucible 440C is a hardenable chromium steel. It has one of the highest attainable hardnesses of the corrosion and heat resisting grades. This grade is magnetic at all times.

Information provided by Crucible Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.276 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 230
Hardness, Rockwell C 59as quenched
 51
@Tempering Temp. 538 °C
 54
@Tempering Temp. 316 °C
 55
@Tempering Temp. 427 °C
 56
@Tempering Temp. 204 °C
 59
@Tempering Temp. 100 °C
Tensile Strength, Ultimate 110 ksi
Tensile Strength, Yield 65.0 ksi
Elongation at Break 14 %in 2"
Reduction of Area 25 %
Modulus of Elasticity 29000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000599 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.70 µin/in-°F
@Temperature 0.000 - 100 °C
 6.00 µin/in-°F
@Temperature 0.000 - 316 °C
Specific Heat Capacity 0.110 BTU/lb-°F
Thermal Conductivity 168 BTU-in/hr-ft²-°F
Melting Point 2500 - 2700 °F
Solidus 1370 °C
Liquidus 1480 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.95 - 1.2 %
Chromium, Cr 16 - 18 %
Iron, Fe >= 79.1 %as balance
Manganese, Mn <= 1.0 %
Molybdenum, Mo <= 0.75 %
Phosphorus, P <= 0.40 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
440C Martensitic Stainless Steel (UNS S44004)
AISI 440 Stainless Steel
Kinetics MIM 440C Stainless Steel
440C Modified Stainless Steel (Composition Spec)
Cast Stainless Steel 440C, ASTM A276

NCRUC908 / 160359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.