MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Veradel® AG-230 Polyethersulfone  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.

Nov. 2009: Veradel® is the replacement trade name for former Radel® R PESU products.

Key Words: PES
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccASTM D792
Water Absorption 0.42 %in 24 hours per ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 126 MPaASTM D638
Elongation at Break 1.9 %ASTM D638
Elongation at Yield 1.9 %ASTM D638
Tensile Modulus 8.62 GPaASTM D638
Flexural Yield Strength 179 MPaASTM D790
Flexural Modulus 8.07 GPaASTM D790
Izod Impact, Notched 0.700 J/cmASTM D256
Tensile Impact Strength 70.0 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 4.1
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
@Thickness 3.30 mm
ASTM D149
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
@Temperature 20.0 °C
ASTM E381
CTE, linear, Transverse to Flow 31.0 µm/m-°C
@Temperature 20.0 °C
ASTM E381
Deflection Temperature at 1.8 MPa (264 psi) 213 °CASTM D648
UL RTI, Electrical 190 °C
@Thickness 1.57 mm
UL RTI, Mechanical with Impact 190 °C
@Thickness 1.57 mm
UL RTI, Mechanical without Impact 190 °C
@Thickness 1.57 mm
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 0.800 mm
 
Compliance PropertiesOriginal ValueComments
USDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos ABS NOVODUR® P3T ABS, Injection Grade
Ineos ABS NOVODUR® P2T ABS, Injection Grade
Mitsubishi Chemical Advanced Materials Semitron™ CMP XL20 PAI
Syensqo (Solvay Specialty Polymers) Veradel® 3300 Polyethersulfone (PESU)
Syensqo (Solvay Specialty Polymers) Kadel® E-1230 Polyketone

PSOLVT14 / 21310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.