MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Glyptal CE237 Enamel
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: GLYPTAL CE-237 GLOSS BLACK is an air-drying or baking enamel. This material has very good oil, chemical, and corrosion resistance. It offers a tough durable film along with excellent arc resistance.

SUGGESTED USES

GLYPTAL CE-237 is designed for the finishing of motor end windings. This material is an offset to 7815 and has improved arc resistance.

APPLICATION

GLYPTAL CE-237 may be applied by spray or dip methods. This material must be kept well agitated during use. Surfaces to be painted should be clean and dry.

Reduction:

Spray: Thin to 25-30 seconds (#2 Zahn Cup) with 1500 Thinner.

Dip: Thin to 23-28 seconds (#2 Zahn Cup) with Solvesso 100.

SURFACE PREPARATION

Surfaces to be painted should be dry and free from dirt, wax, grease, rust, and oil. Remove grease and oil by washing surface with mineral spirits.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 50 %Weight
 
Thermal PropertiesOriginal ValueComments
Flash Point <= 80.0 °F
 
Processing PropertiesOriginal ValueComments
Dry Time 12.0 hourAir Dry: Hard
Tack-Free Time 3.00 hourAir Dry
 
Descriptive Properties
Bake Time10-20 min125°C
 20-30 min95°C
 45-60 min65°C
ColorBlack
Coverage675 ft²/gal1 mil dried film
GlossHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGLYPT927 / 209766

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.