MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Oschatz-Glas HZF 302 Type A/9-272 black Acrylic- Impregnated Glass Filament Thread
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Color coatings are characterized by high UV resistance and good abrasion resistance. The colors used are stable up to a temperature of 180°C and can therefore also be used under high heat influences, e.g. in the cable industry as heat-resistant connecting cables or marking threads.

Information provided by Oschatz-Glas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Loss On Ignition 3.2 - 4.8 %DIN ISO 1887
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °CColor Coating Limit
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ISO 3344
 
Descriptive Properties
Basis MaterialEC 9-272DIN EN 12654
CoatingAcrylic
Colorblack
Linear density of the coated yarn280 tex± 8 %, DIN EN ISO 1889
Spool formatH8-bobbins or H9-bobbins
Tensile strength> 125 NDIN EN ISO 3341

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EOSCH746 / 320727

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.