MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.

Physical properties based on Geon E7506 white 1880.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78ASTM D2240
Tensile Strength, Yield 43.4 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2920 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 84.3 MPaASTM D790
Flexural Modulus 3150 MPaASTM D790
Izod Impact, Notched 110 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Compression Molded; ASTM D256A
Dart Drop Total Energy 57.4 J/cm
@Temperature 23.0 °C
Procedure A, C.125; ASTM D4226
 60.1 J/cm
@Temperature 23.0 °C
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 61.0 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 77.5 °C
@Thickness 3.18 mm
conditioned @ 50 deg.C; ASTM D648
 80.0 °C
@Treatment Temp. 60.0 °C,
Thickness 3.18 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.9 °C
@Thickness 3.18 mm
Compression Molded, Conditioned at 50 deg.C; ASTM D648
 78.3 °C
@Thickness 3.18 mm
Compression Molded, Annealed at 60 deg.C; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 193 - 210 °C
 
Descriptive Properties
FeaturesHigh Gloss
 Medium Impact Resistance
FormsPowder
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
 Extrusion Blow Molding
PVC Cell Classification16354ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesBlow Molding Applications
 Capstock
 Outdoor Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH0POL1387 / 145956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.