MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R 420/50 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: ELASTOSIL® R 420 silicone rubbers feature outstanding tear resistance and high transparency.

Application: In principle ELASTOSIL® R 420 silicone rubbers are designed for extrusion, compression, and transfer and injection molding. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183-1 A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52curing agent E; DIN 53505
 53curing agent C1; DIN 53505
Tensile Strength at Break 10.0 MPacuring agent E; DIN 53504 S1
 11.0 MPacuring agent C1; DIN 53504 S1
Elongation at Break 600 %curing agent E; DIN 53504 S1
 730 %curing agent C1; DIN 53504 S1
Rebound 46 %curing agent C1; DIN 53512
 47 %curing agent E; DIN 53512
Tear Strength 39.0 kN/mcuring agent E; ASTM D624 B
 41.0 kN/mcuring agent C1; ASTM D624 B
Compression Set 23 %
@Temperature 175 °C,
Time 79200 sec
curing agent C1; DIN ISO 815-B
 36 %
@Temperature 175 °C,
Time 79200 sec
curing agent E; DIN ISO 815-B
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Treatment Temp. 135 °C
curing agent E, press cured, 4hr/200°C
 15.0 min
@Treatment Temp. 165 °C
curing agent C1, press cured, 4hr/200°C
 15.0 min
@Treatment Temp. 165 °C
curing agent C6, press cured, 4hr/200°C
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® R plus 4000/50 Silicone Rubber
Dow Silastic® Q7-4750 BIOMEDICAL GRADE ETR ELASTOMER, KIT
Momentive Performance Materials Addisil™ 1050 E Industrial Extrusion Heat Cured Rubber
NuSil MED-2245 Two-Part Standard High Consistency Elastomers - Unrestricted Medical Use
Multibase C6-135 Dow-Corning Class VI Elastomer

PWACK9208 / 204737

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.