MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ TFM™ 2001 Modified PTFE Paste Extrusion Powder  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Extruded

Material Notes: Type I, gr. 2 PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1000. Average particle size 500µm.

Modified PTFE fine powder product for paste extrusion applications. The modified PTFE paste extrusion grade, TFM 2001, combines the traditional attributes of first generation PTFE with benefits such as denser polymer structure and lower permeability; uniform mechanical properties; higher stress cracking resistance; higher pressure resistance under surge stress; and weldability. Dyneon TFM 2001 PTFE is an ideal material for the manufacture of high-performance tubing for hydraulic systems, fuel lines, flexible lines, conveying and transport tubing.

Data provided by Dyneon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.15 g/ccASTM D4895
Apparent Bulk Density 0.450 g/ccDIN 53466
Particle Size 500 µmASTM D4895
Thickness 63.0 mil
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 34.0 MPaASTM D4895
Elongation at Break 400 %ASTM D4895
 
Descriptive Properties
Extrusion Pressure3770 psireduction ratio 400; ASTM D4895
Reduction Ratio Range20-1000:1Dyneon Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE 62 Resin for Lubricated Paste Extrusion
Chemours Teflon® PTFE 7A Granular Molding Powder
Chemours Teflon® PTFE 60 Resin for Lubricated Paste Extrusion
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
3M Dyneon™ TFM™ 2001Z PTFE

PDYM20 / 34660

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.