MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ PC 8701-15 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: EMERGE™ PC 8701 advanced resin is an ignition-resistant, 10% glass reinforced polycarbonate resin. This resin contains no bromine, chlorine or phosphate additives. It is a medium flow PC resin with a mold release system, intended for applications requiring high stiffness. It has a UL94 flammability rating of V-0 at 1.5 mm.

Main Characteristics:

  • Glass reinforced
  • Ignition resistant
Applications:
  • Powered Device Housings
  • Information technology equipment
  • Electrical parts
  • Other structural/internal parts

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccISO 1183/B
Linear Mold Shrinkage 0.0040 - 0.0060 in/inISO 294-4
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Tensile Strength, Yield 65.0 MPa
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Elongation at Break 9.0 %
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Elongation at Yield 4.0 %
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Tensile Modulus 3950 MPa
@Thickness 4.00 mm
Injection Molded; ISO 527-2/1
 4000 MPa
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Flexural Strength 105 MPa
@Thickness 4.00 mm
Injection Molded, 2.0 mm/min; ISO 178
Flexural Modulus 3800 MPaInjection Molded, 2.0 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²Injection Molded; ISO 180/A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 50 Hz
IEC 60250
 3.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength >= 70.0 kV/mmIEC 60243-1
Dissipation Factor 0.016
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 V
@Thickness 3.00 mm
Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature -40.0 - 80.0 °C
ASTM D696
Hot Ball Pressure Test >= 125 °CIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 141 °CAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 133 °CUnannealed; ISO 75-2/A
 139 °CAnnealed; ISO 75-2/A
Vicat Softening Point 145 °CISO 306/B50
 155 °CISO 306/A120
Flammability, UL94 V-0
@Thickness 1.50 mm
Oxygen Index 29 %ISO 4589-2
Glow Wire Ignition Temperature 960 °C
@Thickness 1.00 mm
IEC 60695-2-13
 960 °C
@Thickness 2.00 mm
IEC 60695-2-13
 960 °C
@Thickness 3.00 mm
IEC 60695-2-13
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 - 315 °C
Mold Temperature 80.0 - 115 °C
Drying Temperature 120 °C
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo EMERGE™ PC 8702-15 (AP) Polycarbonate Resin
Trinseo EMERGE™ 8702 Polycarbonate
Trinseo EMERGE™ 8600-20 Polycarbonate
Mitsubishi Novaduran® 5010CTN33 Polybutylene Terephthalate
Trinseo EMERGE™ PC 8130-15 Polycarbonate Resin

PTRINS9047 / 197546

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.