MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 3762 Polypropylene, Extrusion Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Homopolymer fiber grade for staple fiber and multifilament yarns

Fading Resistance - FINA 3762 is formulated to resist gas fading while maintaining excellent processing stability up to 250oC.

Process Stability - FINA 3762 features excellent processability and the good physical properties necessary for fibers and multifilaments.

FDA - FINA 3762 complies with all applicable FDA regulations for food contact.

Recommended Applications - FINA 3762 is recommended for staple fibers and bulk continuous filament (BCF) yarns.

Processing - FINA 3762 resin processes on conventional extrusion equipment with typical melt temperatures of 400-480°F (204- 250°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 18 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 250 MPaFiber value estimated from tenacity; ASTM D3218
Elongation at Break 65 %Fiber property, 1.5 dpf multifilament. ASTM D3218
Modulus of Elasticity 1.65 GPaASTM D638
Tenacity 3.20 g/denierASTM D3218
Flexural Modulus 1.515 GPaFlexural modulus is 1.515 GPa. Flexural stiffness is 1.215 GPa. ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
Vicat Softening Point 150 - 155 °CSoftening point range is 150-155°C. Method not specified.
 
Processing PropertiesOriginal ValueComments
Melt Temperature 204 - 250 °CExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape
Total PPH 4030 Polypropylene Homopolymer
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer
Overview of materials for Polypropylene with 30% Glass Fiber Filler

PFIN28 / 38358

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.