MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos R35C-00 Polypropylene Random Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Grade R35C-00 is a high clarity random copolymer with a high flow rate. This material is designed for high speed injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

Applications

  • Consumer products
  • Housewares
  • Medical
  • Thin-wall rigid packaging
Benefits
  • Excellent clarity
  • Rapid cycle times
  • Good molding performance in thin-wall parts
  • Good impact resistance at room and refrigerator temperatures

Key Words: High clarity, high flow rate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.903 g/ccASTM D792
Melt Flow 55 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 83Injection Molded; ASTM D785
Tensile Strength at Break 3530 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 4060 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break >= 800 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 13 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 149000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 0.400 ft-lb/in
@Temperature 3.89 °C
Injection Molded; ASTM D256
 0.770 ft-lb/in
@Temperature 22.8 °C
Injection Molded; ASTM D256
Izod Impact, Notched (ISO) 0.999 ft-lb/in²
@Temperature 3.89 °C
Area; ASTM D256
 1.90 ft-lb/in²
@Temperature 22.8 °C
Area; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 185 °FUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 237 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 16.5 %
@Thickness 1.27 mm
ASTM D1003
Gloss 91 %60°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos R35C-01 Polypropylene Random Copolymer
Ineos H01H-00 Polypropylene Homopolymer
Ineos R12C-00 Polypropylene Random Copolymer
Ineos R12C-01 Polypropylene Random Copolymer
Ineos R01C-00 Polypropylene Random Copolymer

PINEOS014 / 48182

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.