MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C50580, OS015 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Nominal Grain Size 0.015 mm

Excellent Suitability – Soldering, Brazing, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Gas Shielded Arc Welding, Spot Weld, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding, Coated Metal Arc Welding, Seam Weld

Applicable Specifications: Strip – ASTM B888/B88M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.321 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 53.0 ksi
Tensile Strength, Yield 29.0 ksi0.2% Offset
Elongation at Break 50 %
Tensile Modulus 17000 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.33Calculated
Machinability 20 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000420 ohm-cm41% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.90 µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity 130 BTU-in/hr-ft²-°F
Melting Point 1900 - 1970 °F
Solidus 1900 °F
Liquidus 1970 °F
Annealing Point 700 - 1350 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 97.2 - 98.9 %As Balance
Iron, Fe 0.050 - 0.20 %
Lead, Pb <= 0.050 %
Nickel, Ni 0.050 - 0.20 %
Phosphorus, P 0.010 - 0.35 %
Tin, Sn 1.0 - 1.7 %
Zinc, Zn <= 0.30 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC50580x6 / 292100

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.