MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Potters Industries EMB-10 Low Alkaline BorosilicateGlass
Categories: Ceramic; Glass

Material Notes: SPHERIGLASS® Solid Glass Microspheres have been developed as filler for paints, coatings and films. A key feature of this product is the low alkalinity of the spheres.

Features:

  • Good fluidity and dispersion
  • Isotropic fillers cause no strain
  • Low alkaline solubility
Applications
  • Hardness improvement
  • Surface matting
  • High Abrasion Performance
  • High Heat Resistance
  • Anti-blocking

Information provided by Potters Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
Particle Size 5.0 µmMean
 2.0 - 10 µmRange
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 6.5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.10 µm/m-°C
Specific Heat Capacity 0.836 J/g-°C
Thermal Conductivity 1.03 W/m-K
Softening Point 830 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53 - 1.57
 
Component Elements PropertiesOriginal ValueComments
Al2O3 14 %
B2O3 5.7 %
CaO 23.1 %
Fe2O3 0.20 %
MgO 1.0 %
Na2O or K2O 0.50 %
SiO2 55.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borosilicate Glass, Low Expansion
Potters Industries EMB-20 Low Alkaline BorosilicateGlass
Corning 7761 Potash Borosilicate Crushed/Powdered Glass
Corning 7056 Alkali Borosilicate Crushed/Powdered Glass
Borosilicate Glass

CPOT8002 / 184628

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.