MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Kalrez® 9100 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DuPont™ Kalrez® 9100 perfluoroelastomers parts are an amber translucent product for PV cell manufacturing processes requiring resistance to fluorine-based plasma including amorphous/microcrystalline silicon thin film deposition. It exhibits very low weight loss and ultra-low particle generation in fluorine-based plasma, e.g., NF3, F2, etc. It also offers excellent resistance to dry process chemistry and has excellent thermal stability, compression set and outgassing properties. Kalrez® 9100 has good mechanical strength properties and is well suited for both static and dynamic sealing applications. A maximum continuous service temperature of 300 °C is suggested.

Features/Benefits

  • Very low weight loss and ultra-low particle generation in fluorine-based plasma
  • Excellent resistance to dry process chemistry
  • Excellent thermal stability
  • Excellent (low) compression set and outgassing properties

Suggested Applications

  • Gas valve/slit valve door seals
  • Gas inlet/orifice seals
  • Isolation valve seals
  • Substrate handling pads
  • Chamber lid seals

Information provided by DuPont

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D 2240
Elongation at Break 238 %238 %ASTM D 412
100% Modulus 5.20 MPa754 psiASTM D 412
 
Thermal PropertiesMetricEnglishComments
CTE, linear 464 µm/m-°C258 µin/in-°FISO 11359-1/-2
Maximum Service Temperature, Air 300 °C572 °FDuPont proprietary test
Minimum Service Temperature, Air -3.15 °C26.3 °FRetraction temperature TR-10; ASTM D 1329
 
Descriptive Properties
ColorAmber
Polymer(FFKM)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® 4079 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 4079AMS FFKM Perfluoroelastomer
Lotte Advanced Materials Starex® WR-9100 ASA, Unreinforced
DuPont Mobility and Materials Kalrez® 7075 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 8575 FFKM Perfluoroelastomer

PDVC9788 / 170429

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.