MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Die Cast
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Used in bearing applications. ZA-27 has a higher bearing load capacity than bronze bearing alloys, although its environment (both temperature and corrosive) is more limited.

Key Words: Zinc Foundry Alloy; UNS Z35841 (Castings); UNS Z35840 (Ingot)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.02 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 119500 kg load; 10 mm hardened steel ball
Hardness, Knoop 120Estimated from Brinell Value
Hardness, Rockwell A 40Estimated from Brinell Value
Hardness, Rockwell B 60Estimated from Brinell Value
Hardness, Vickers 107Estimated from Brinell Value
Tensile Strength, Ultimate 426 MPa
@Diameter 6.35 mm
Tensile Strength, Yield 371 MPa
@Strain 0.2 %
Elongation at Break 2.5 %in 5 cm
Modulus of Elasticity 77.9 GPa
Compressive Strength 359 MPa0.1% offset
Fatigue Strength 117 MPa
@# of Cycles 5.00e+8
Reverse Bending
Shear Strength 325 MPa
Charpy Impact, Unnotched 12.0 J
@Thickness 6.35 mm
square bar
Coefficient of Friction 0.030 - 0.070
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000580 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 128 J/g
CTE, linear 26.0 µm/m-°C
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.525 J/g-°C
Thermal Conductivity 125 W/m-K
Melting Point 376 - 484 °C
Solidus 376 °C
Liquidus 484 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 515 - 545 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 25 - 28 %Addition, Casting
 25.5 - 28 %Addition, Ingot form
Cadmium, Cd <= 0.0050 %Impurity, Ingot form
 <= 0.0060 %Impurity, Casting
Copper, Cu 2.0 - 2.5 %Addition, Casting
 2.0 - 2.5 %Addition, Ingot form
Iron, Fe <= 0.072 %Impurity, Ingot form
 <= 0.075 %Impurity, Casting
Lead, Pb <= 0.0050 %Impurity, Ingot form
 <= 0.0060 %Impurity, Casting
Magnesium, Mg 0.010 - 0.020 %Addition, Casting
 0.012 - 0.020 %Addition, Ingot form
Tin, Sn <= 0.0020 %Impurity, Ingot form
 <= 0.0030 %Impurity, Casting
Zinc, Zn 69.396 - 72.488 %As balance; Ingot per ASTM B 669
 69.39 - 72.99 %As balance; Castings per ASTM B 791
 
Descriptive Properties
Damping10.9 Q-1 x 103at 100 Hz, 100°C
 5 Q-1 x 103at 100 Hz, 20°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Die Cast
Zinc ZA-8 (Zn-8Al-1Cu-0.02Mg), Die Cast
Zinc AC43A (Zinc Alloy 2; Zn-4Al-2.5Cu-0.04Mg; Number 2 Die Casting Alloy; Zamak 2), Die Cast
Aluminum 384.0-F Die Casting Alloy
Zinc AC41A Alloy (Zamak 5), As Cast

MZN27C / 14522

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.