MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KiON ANTI-GRAFFITI CLEAR COAT Ambient Cure, Polysilizane Clear Coat  (discontinued **)
Categories: Fluid; Polymer; Thermoset

Material Notes: KiON Anti-Graffiti Clear Coat is a clear, ready-to-use Polysilazane clear coat that can be used to resist graffiti, road tar, tree sap, dirt, grease, stains and the like. KiON Anti-Graffiti Clear Coat will cure at ambient temperature and is dry-to-touch within 1 hour of application. KiON Anti-Graffiti Clear Coat can easily be applied by spraying, dipping, or brush coating. Resistance to most graffiti insults (permanent marker, etc.) can be obtained after a two day cure and full anti-graffiti protection against spray paint can be obtained after a 7 day cure. Dried spray paint can be removed from surfaces coated with KiON Anti-Graffiti Clear Coat by mild mechanical abrasion or spray washing. In addition, KiON Anti-Graffiti Clear Coat has excellent “weatherability”, UV resistance, hardness, and abrasion resistance, as well as oxidation and corrosion resistance.

Applications

Suggested major applications include but are not limited to transportation, highway signage, and building facades.

Information provided by KiON Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.904 g/ccLiquid
Volatile Organic Compounds (VOC) Content 659 g/l
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 26.0 °C
 
Descriptive Properties
%Resin23.7 wt% solids
Adhesion ASTM D 335990-100% on chromated aluminum
AppearanceClear, colorless
Chemical ResistanceMEK, Acetone, Brake Fluid, and most organic solvents
Pencil Hardness ASTM D 33636H on chrome treated aluminum
UV StabilityExcellent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKION09 / 48725

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.