MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-901 Fluoroelastomer Terpolymer, 71% Fluorine Content  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-901 is a terpolymer suitable for various peroxide cure systems. DAI-EL® G-901 can be formulated to eliminate the post cure process. DAI-EL® G-901 is suitable for transfer and compression molding applications requiring excellent chemical and steam resistance.

Typical Applications: O-Rings, gaskets and seals

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.91 g/cc
Mooney Viscosity 48
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
 72
@Treatment Temp. 232 °C,
Time 252000 sec
Air Oven Aging
Tensile Strength at Break 22.9 MPa
 19.7 MPa
@Treatment Temp. 200 °C,
Time 252000 sec
Air Oven Aging
Elongation at Break 300 %
 348 %
@Treatment Temp. 200 °C,
Time 252000 sec
Air Oven Aging
100% Modulus 5.00 MPa
@Strain 100 %
Compression Set 32 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring; ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -8.00 °CLow Temperature Retraction, TR10
Brittleness Temperature -26.0 °CEmbrittlement
 
Processing PropertiesOriginal ValueComments
Cure Time 0.900 mints2, scorch time
 1.20 mint'50, time to 50% cure
 1.70 mint'90, time to 90% cure
 4.00 hour
@Temperature 200 °C
Post cure
 10.0 min
@Temperature 177 °C
Press Cure
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 71 %
 
Descriptive Properties
ColorWhite to light pink
MH26.9 dNmmaximum torque
ML0.6 dNmminimum torque
Test Formula100 phrDAI-EL® G-901
 3 phrPeroxide (50% Activity)
 3 phrZinc Oxide
 30 phrMT Carbon Black (N-990)
 4 phrTAIC (72% Activity)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin DAI-EL® G-901 Fluoroelastomer Terpolymer, 70.5% Fluorine Content

PDAIJ9857 / 209928

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.