MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Wacker® Silane P-TRIETHOXY
Categories: Fluid

Material Notes: Structural formula: C6H5Si(OCH2CH3)3

Empirical formula: C12H20O3Si

CAS No.: 780-69-8

Product description: Colorless, clear liquid with a weak characteristic odor. Soluble in organic solvents; not in water.

Properties: WACKER® SILANE P-TRIETHOXY offers the following performance advantages:

  • Increased yield of polymer per unit weight of catalyst.
  • Increased isotactic content of polypropylene-based polymers.
  • Improved molecular weight dispersity of the polymer.
Application: WACKER® SILANE P-TRIETHOXY is used as component of a Ziegler-Natta olefin polymerization catalyst system.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/ccDIN 51757
Viscosity 1.6 cPdynamic; DIN 51562
Molecular Weight 240.4 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 235 °C
@Pressure 0.1013 MPa
Flash Point >= 40.0 °CISO 2719
Ignition Temperature 265 °CDIN 51794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46
 
Descriptive Properties
Content<20 mg/kgHydrolyzable chloride
Purity>98%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Vistamaxx™ 8880 Performance Polymer
Wacker Wacker® Silane CP2-DIMETHOXY
LyondellBasell Akoalit PB 4237 grey Polyolefin

PWACK9814 / 205343

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.