MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long term exposure to temperatures from -60° to +500°F is required. lt is 100% reactive and does not contain any solvents or diluents. It is formulated to cure rapidly at elevated temperatures. It has a convenient 100 to 30 mix ratio, by weight. It produces high strength bonds at both ambient and elevated temperatures. Master Bond EP45HTQ can be applied without sagging or dripping on vertical surfaces. It produces durable high strength and tough bonds which are remarkably resistant to thermal cycling and chemicals including water, oil and most organic solvents over the exceptionally wide temperature range of - 60°F to more than +500°F. It also produces superior seals & high quality pottings. Adhesion to metals, glass, ceramics, wood, vulcanized rubber and many plastics is excellent. The hardened compound is an electrical insulator. Color of Part A is tan, part B is tan. Master Bond EP45HTQ is widely used in aerospace, electronic, electrical, computer, construction, metal working, appliance, automotive and chemical industries.

Product Advantages:

  • Convenient mixing: 100/30 mix ratio by weight
  • Easy application: contact pressure only required for cure, compound spreads evenly and smoothly; no drip application feature
  • Convenient cure schedules: long pot life at room temperature, requires elevated temperature cure.
  • High bonding strength to similar and dissimilar substrates
  • Superior durability, thermal shock and chemical resistance
  • Reactive and does not contain any solvents or diluents
  • Resists ETO sterilization, chemical sterilants and repeated autoclaving
  • High compressive strength
  • Resistance to radiation up to 10^10 rads

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 80
Tensile Strength at Break >= 11000 psi
Elongation at Break >= 5.0 %
Tensile Modulus 500000 psi
Compressive Strength >= 19000 psi
Shear Strength >= 2300 psiBond, Al to Al
Peel Strength >= 12.0 pliT-peel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 - 30.0 µm/m-°C
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 135 - 163 °C
Pot Life >= 720 min200 gram batch
 >= 720 min1 quart mass
Shelf Life 6.00 Month
 
Descriptive Properties
Mixing Ratio (A to B)100/30by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP46HT-1 Epoxy For High Temperature Service
Hexcel® Redux® 308 Modified epoxy film adhesive
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy
Dymax 4-425 Glass Bonding Adhesive
Dow 733 GLASS & METAL SEALANT

PMASTB405 / 149652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.