Hostacom EYC 136N T 1064 is a 13% talc filled PP copolymer, with excellent flowability, high stiffness, and excellent scratch resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 1064 color version. Applications: Interior TrimsInformation provided by LyondellBasell. |