MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil EXACT™ 4150 Plastomer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO), Film Grade; Polyethylene (PE)

Material Notes: Product Description: Exact 4150 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4150 is designed for multilayer coextruded cast film applications requiring low sealing temperatures, high oxygen transmission, and high toughness. Typical applications include seal layers for lamination films used in meat, poultry, and fresh produce packaging.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Cast Film
  • Lamination Film

Data provided by the manufacturer, Exxon Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.895 g/ccExxon Method
Thickness 0.800 mil
Melt Flow 3.5 g/10 minExxon Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 4.76 MPaASTM D882
Film Tensile Strength at Yield, TD 4.21 MPaASTM D882
Film Elongation at Break, MD 470 %ASTM D882
Film Elongation at Break, TD 660 %ASTM D882
Film Elongation at Yield, MD 10 %ASTM D882
Film Elongation at Yield, TD 9.0 %ASTM D882
Secant Modulus, MD 0.0552 GPaASTM D882
Secant Modulus, TD 0.0593 GPaASTM D882
Puncture Energy 47.0 in-lbExxonMobil Method
Elmendorf Tear Strength, MD 200 g/milASTM D1922
Elmendorf Tear Strength, TD 438 g/milASTM D1922
Dart Drop 675 g/milASTM D1709
Film Tensile Strength at Break, MD 75.8 MPaASTM D882
Film Tensile Strength at Break, TD 68.9 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 89.0 °CExxon Method
Crystallization Temperature 162 °CExxonMobil Method
Vicat Softening Point 167 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 0.10 %ASTM D1003
Gloss 97 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force12 lbfExxonMobil Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lucalen A2920M Low Density Polyethylene
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
Celanese 191A LDPE polymer for adhesives, automotive and compounds
ExxonMobil Escorene® LD 713.93 Cast Film Resin
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin

PEXCIF / 38035

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.