MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celstran® PP-GF40-04 natural PP, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes:

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psi5mm/min; ISO 527-2/1A
Tensile Strength 75.0 MPa
@Temperature 80.0 °C
10900 psi
@Temperature 176 °F
ISO 527-1, -2
Elongation at Break 2.0 %2.0 %5mm/min
 2.3 %
@Temperature 80.0 °C
2.3 %
@Temperature 176 °F
ISO 527-1, -2
Tensile Modulus 9.20 GPa1330 ksi50mm/min; ISO 527-2/1A
 6.20 GPa
@Temperature 80.0 °C
899 ksi
@Temperature 176 °F
ISO 527-1, -2
Flexural Strength 200 MPa29000 psiISO 178
 120 MPa
@Temperature 80.0 °C
17400 psi
@Temperature 176 °F
ISO 178
Flexural Modulus 9.00 GPa1310 ksiISO 178
 6.40 GPa
@Temperature 80.0 °C
928 ksi
@Temperature 176 °F
ISO 178
Charpy Impact Unnotched 6.20 J/cm²29.5 ft-lb/in²ISO 179/1eU
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²11.9 ft-lb/in²ISO 179/1eA
 3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 162 °C324 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 158 °C316 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 128 °C262 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 270 °C446 - 518 °Fhot runner
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 220 - 230 °C428 - 446 °F
Zone 2 230 - 240 °C446 - 464 °F
Zone 3 240 - 250 °C464 - 482 °F
Zone 4 250 - 260 °C482 - 500 °F
Die Temperature 240 - 250 °C464 - 482 °F
Melt Temperature 250 °C482 °FISO 294
 230 - 270 °C446 - 518 °F
Mold Temperature 70.0 °C158 °FISO 294
Injection Velocity 80.0 mm/sec3.15 in/secISO 294
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.20 %<= 0.20 %
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 40.0 - 80.0 MPa5800 - 11600 psi
 83.0 MPa12000 psiISO 294
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed 25 rpm
@Diameter 75.0 mm
25 rpm
@Diameter 2.95 in
 
Descriptive Properties
Heat stabilized/stable to heatYes
Injection moldingYes
Injection speedslow
Sheet extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PP-GF40-04 Black PP, 40% Glass Reinforced
Envalior Akulon® K224-G6-FC NA99001 PA6-GF30, Dry, 30% Glass Filled
Techmer ES HiFill® PP LGF40 CC HS BK 40% Glass Filled
Niche Polymer POLIXL™ PPHGF40BK PPH, 40% Fiberglass Reinforced
Mocom (ALBIS) Altech® NXT PP PP-H A 2040/456.01 LE GF40 CP 40% Glass Filled PP Homopolymer

PHCQ221B / 183212

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.