MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epoxies, Etc 50-3185 NC, Catalyst #190 Thermally Conductive Potting & Encapsulating Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Description: 50-3185 NC is a filled epoxy encapsulant possessing excellent physical, electrical, and thermal properties. 50-3185 NC is an excellent choice where low thermal expansion, outstanding electrical insulation and/or high thermal conductivity is required. Three catalysts are available to choose from. When cured with Catalyst 190 or Catalyst 30 this system meets NASA’s outgassing requirements.

Features:

  • Low Thermal Expansion
  • Excellent Electrical Insulator
  • High Thermal Conductivity
  • Protects & Conceals Circuitry
Applications: 50-3185 NC is ideal for high voltage applications such as power supplies, transformers, high voltage insulators, bushings, etc

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.31 g/cc
Water Absorption 0.010 %
@Time 86400 sec
Viscosity 16800 cP
Linear Mold Shrinkage 0.0040 in/in
Outgassing - Total Mass Loss 0.020 %CVCM
 0.75 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 96
Flexural Strength 15000 psi
Compressive Strength 24000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.90e+16 ohm-cm
Dielectric Constant 5.21
@Frequency 1e+6 Hz
Dielectric Strength 390 V/mil
Dissipation Factor 0.036
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 29.7 µm/m-°C
Glass Transition Temp, Tg 77.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX058 / 316735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.