MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Flex® TPE G 7150 BLK
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Multi-Flex® G 7150 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactured by Shell, under the reference Kraton G 7150 and complies to the internal specifications of Shell/Multibase. The burn rate is 0.7 in/min (217.5 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.

Data provided by Multibase.

Key Words: Thermoplastic Elastomer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/ccASTM D792
Linear Mold Shrinkage 0.010 cm/cmASTM D955
Melt Flow 5.0 g/10 min(Condition L) ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8910 sec; ASTM D-2240
Tensile Strength, Ultimate 4.80 MPaASTM D412
Elongation at Break 450 %ASTM D412
Flexural Modulus 0.110 GPamethod 1, Proc.B; ASTM D-790
Tear Strength 29.8 kN/mASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Multibase Multi-Flex® TPE G 7455 BLK
Multibase Multi-Flex® TPE G 7821
Multibase Multi-Flex® TPE D 4701 GREY
Multibase Multi-Pro® 4009 T Polypropylene
Multibase Multi-Flex® TPE G 7940 GRAPHITE

PLA118 / 49579

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.