MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® 70G35HSRX BK099 PA66-GF35  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: 35% Glass Reinforced, Heat Stabilized, Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccDAM; ISO 1183
Melt Density 1.24 g/cc
@Temperature >=261 °C
Water Absorption 5.5 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.70 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 285 MPaH 961/30; ISO 2039-1
Tensile Strength at Break 150 MPa50% RH; ISO 527-1/-2
 230 MPaDAM; ISO 527-1/-2
Elongation at Break 3.5 %DAM; ISO 527-1/-2
 5.5 %50% RH; ISO 527-1/-2
Tensile Modulus 9000 MPa50% RH; ISO 527-1/-2
 12000 MPaDAM; ISO 527-1/-2
Flexural Modulus 9.00 GPa50% RH; ISO 178
 13.0 GPaDAM; ISO 178
Poissons Ratio 0.33DAM; ISO 527-1/-2
 0.3450%RH; ISO 527-1/-2
Izod Impact, Unnotched (ISO) 12.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 15.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 13.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Puncture Energy 6.00 J
@Temperature 23.0 °C
DAM; ISO 6603-2
Tensile Creep Modulus, 1 hour 8500 MPa50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 6500 MPa50% RH; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cm50% RH; IEC 62631-3-1
 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 1.00e+13 ohm50% RH; IEC 62631-3-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 17.0 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 85.0 µm/m-°CDAM; ISO 11359-1/-2
Specific Heat Capacity 2.13 J/g-°C
@Temperature >=261 °C
Melt
Thermal Conductivity 0.240 W/m-K
@Temperature >=261 °C
Melt
Melting Point 261 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 252 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 20.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 70.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 0.700 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread 26.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 21 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 285 - 305 °CInjection
 295 °CInjection Optimum
Mold Temperature 70.0 - 120 °CInjection
 100 °CInjection Optimum
Ejection Temperature 210 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %Injection
Hold Pressure 50.0 - 100 MPaInjection
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging G-value (condensate) (mg)0.5ISO 6452; DAM
Hold pressure time (s/mm)3Injection
Max. screw tangential speed (m/s)0.2Injection
Odor3VDA 270
Part Marking CodePA66-GF35ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA66-GF35ISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 70G35HSL NC010 PA66-GF35
Celanese Zytel® 103FHSA NC010 PA66
Celanese Zytel® 70G35EF NC010 PA66-GF35
Celanese Zytel® 70G35HSLRA4 BK267 PA66-GF35
Celanese Zytel® 70G35HSLX BK357 PA66-GF35

PDSX5340 / 197980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.