MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® E62-S3 BK V303579 Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® E62-S3 BK V303579 is a PA 12 elastomer consisting of PA 12 segments and softening segments. The material is free of volatile or migrating plasticizer. The VESTAMID® E represent thermoplastic elastomers generically characterized as polyether block copolyamides (PEBA) consisting of PA 12 and polyether segments. VESTAMID® E62-S3 BK V303579 is especially developed for sport shoe soles. It has good impact strength at low temperatures. VESTAMID® E62-S3 BK V303579 is supplied as cylindrical pellets in moisture-proof packaging, ready for processing. The process temperatures should be within a range of 190°C – 230°C. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Automotive and Mobility, Sustainable, Industry and Engineering, Sports and Lifestyle
Sustainability: Sustainable electricity
Delivery form: Pellets, Granules
Optics: Translucent
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Unfilled
Special Characteristics: Light-stabilized, High heat resistant
Color: Black
Additives: Heat stabilizer

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 9.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 61.0
@Time 3.00 sec
61.0
@Time 0.000833 hour
ISO 7619-1
Tensile Strength at Break 42.0 MPa6090 psiISO 527
Tensile Strength 24.0 MPa3480 psiISO 527
Tensile Stress 37.4 MPa5420 psiTPE; ISO 527
 15.3 MPa
@Strain 5.00 %
2220 psi
@Strain 5.00 %
ISO 527
 20.4 MPa
@Strain 10.0 %
2960 psi
@Strain 10.0 %
ISO 527
 23.0 MPa
@Strain 50.0 %
3340 psi
@Strain 50.0 %
ISO 527
 23.2 MPa
@Strain 20.0 %
3360 psi
@Strain 20.0 %
ISO 527
 23.3 MPa
@Strain 50.0 %
3380 psi
@Strain 50.0 %
ISO 527
 26.8 MPa
@Strain 100 %
3890 psi
@Strain 100 %
ISO 527
Tensile Strength, Yield 24.0 MPa3480 psiISO 527
Elongation at Break 194 %194 %TPE; ISO 527
 320 %320 %Nominal; ISO 527
Elongation at Yield 30.0 %30.0 %ISO 527
Tensile Modulus 0.405 GPa58.7 ksiISO 527
Charpy Impact, Notched 9.50 J/cm²45.2 ft-lb/in²Type of failure: P; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 171 °C340 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 °C428 °FInjection Molding; ISO 294
Mold Temperature 35.0 °C95.0 °FInjection Molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption14.7 kgISO 14040, 14044
ColorBlack
Global Warming Potential1.8 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 6.3 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 6.3 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.2 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7898 / 325030

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.