MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cyclopentane, C5H10
Categories: Fluid; Solvent

Key Words: C5H10
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.745 g/cc
@Temperature 20.0 °C
Viscosity 0.428 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 70.135 g/mol
Vapor Pressure 256.693 torr
@Temperature 20.0 °C
Surface Tension 22.61 dynes/cm
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 44.5 atm
Critical Temperature 239 °C
Critical Density 0.270 g/cc
Critical Molar Volume 260 cm³/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 389.2 J/g
Specific Heat Capacity 1.182 J/g-°C
@Temperature 25.0 °C
Vapor
Thermal Conductivity 0.1266 W/m-K
@Temperature 20.0 °C
Melting Point -93.9 °C
Boiling Point 49.3 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.407
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.8574
Antoine's Vapor Pressure B Parameter2558.48
Antoine's Vapor Pressure C Parameter-41.79
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)287-92-3
Chemical FormulaC5H10
Critical Compressibility (Zc)0.276
Dipole moment (p/C.m)none
Henry's Law Constant (atm m3/mol)0.188
Molar Heat Capacity (298K)82.876 J/mol-K
Molar Heat Capacity of Vapor a Parameter-53.5887
Molar Heat Capacity of Vapor b Parameter0.5422
Molar Heat Capacity of Vapor c Parameter-0.0003029
Molar Heat Capacity of Vapor d Parameter6.451E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number2246
UV cut-off (nm)210

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nye Lubricants 5200 (SVLG) Synthetic Oil

VORGS089 / 99472

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.