MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shandong Rike Chemical HELI™ HL-2005 Weather-resistance Acrylic Impact Modifier (AIM)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: This PVC impact modifier is an acrylic copolymer (ACR) with a core-shell structure. The cores are acrylic ester and shells are methacrylic copolymers. The basic function of this impact modifier is to improve the impact performance of PVC products to meet the requirements of engineering plastics and simultaneously increase their heat and light stability.

Information Provided by Shandong Rike Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Izod Impact, Unnotched (ISO) 14.6 kJ/m²
@Temperature 0.000 °C
Phr = 0
 19.1 kJ/m²
@Temperature 0.000 °C
Phr = 5
 19.7 kJ/m²
@Temperature 23.0 °C
Phr = 0
 25.3 kJ/m²
@Temperature 0.000 °C
Phr = 8
 34.7 kJ/m²
@Temperature 23.0 °C
Phr = 5
 37.1 kJ/m²
@Temperature 23.0 °C
Phr = 8
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 84.6 °CPhr = 8
 86.0 °CPhr = 0
 
Descriptive Properties
Light Aging - Whiteness Variation (%)15.3Phr = 8
 17.1Phr = 5
 51.22Phr = 0
Thermal Aging - Whiteness Variation (%)20.4Phr = 0
 26.8Phr = 5
 31.1Phr = 8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSHAN009 / 103399

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.