MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nabaltec NABALOX® NO 115-25 Ground Alumina
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: NABALOX® aluminum oxide has a number of advantages including
  • low sintering temperature
  • wide sintering range
  • flexible processing
  • high sintered densities high wear and impact resistance
  • electrical insulation
  • high mechanical strength
  • high temperature properties
  • dimensional accuracy
  • optimized chemical resistance

Refractory Industry, Wear-resistant ceramics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 - 0.900 g/cc
Density 2.29 g/ccGreen Density
 3.10 g/ccSintered Density
 3.90 g/cc
Loss On Ignition <= 0.30 %
@Temperature 20.0 - 1100 °C
Particle Size >= 2.0 µmPrimary Crystal Size
 4.0 µmMedian Grain Diameter
Specific Surface Area 0.70 - 1.5 m²/gBET
 
Thermal PropertiesOriginal ValueComments
Shrinkage 12 %Sintering Shrinkage
 
Processing PropertiesOriginal ValueComments
Sintering Temperature 1750 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 98 %alpha-Al2O3
 >= 99.6 %
Fe2O3 0.030 %
Na2O 0.30 %
SiO2 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nabaltec NABALOX® NO 105 Calcined Aluminum Oxide
Nabaltec APYRAL® AOH 60 AlO(OH) Boehmite
Nabaltec APYRAL® AOH 20 AlO(OH) Boehmite
Nabaltec NABALOX® NO 315 Ground Alumina
Nabaltec NABALOX® NO 313 Ground Alumina

CNABAL37 / 54562

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.