MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haynes 25 alloy, cold worked sheet, 10% cold reduction
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal galling. Applications in the aerospace industry, including parts in military and commercial gas turbine engines.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: UNS R30605, AMS 5537, AMS 5759, AMS 5796, AMS 5795
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 9.13 g/ccat RT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1070 MPa
 270 MPa
@Temperature 980 °C
 425 MPa
@Temperature 870 °C
 600 MPa
@Temperature 760 °C
 785 MPa
@Temperature 540 °C
 795 MPa
@Temperature 650 °C
Tensile Strength, Yield 725 MPa
@Strain 0.2 %
 185 MPa
@Strain 0.2 %,
Temperature 980 °C
 325 MPa
@Strain 0.2 %,
Temperature 870 °C
 460 MPa
@Strain 0.2 %,
Temperature 760 °C
 540 MPa
@Strain 0.2 %,
Temperature 540 °C
 550 MPa
@Strain 0.2 %,
Temperature 650 °C
Elongation at Break 41 %in 51 mm
 8.0 %
@Temperature 760 °C
in 51 mm
 13 %
@Temperature 870 °C
in 51 mm
 15 %
@Temperature 980 °C
in 51 mm
 37 %
@Temperature 650 °C
in 51 mm
 48 %
@Temperature 540 °C
in 51 mm
Reduction of Area 41 %
 8.0 %
@Temperature 760 °C
 13 %
@Temperature 870 °C
 15 %
@Temperature 980 °C
 37 %
@Temperature 650 °C
 48 %
@Temperature 540 °C
Modulus of Elasticity 225 GPaRT
 146 GPa
@Temperature 1000 °C
 154 GPa
@Temperature 900 °C
 163 GPa
@Temperature 800 °C
 174 GPa
@Temperature 700 °C
 181 GPa
@Temperature 600 °C
 188 GPa
@Temperature 500 °C
 197 GPa
@Temperature 400 °C
 204 GPa
@Temperature 300 °C
 214 GPa
@Temperature 200 °C
 222 GPa
@Temperature 100 °C
Charpy Impact 262 J
 144 J
@Temperature 980 °C
 148 J
@Temperature -196 °C
 163 J
@Temperature 870 °C
 182 J
@Temperature -138 °C
 194 J
@Temperature 760 °C
 212 J
@Temperature -78.0 °C
 230 J
@Temperature 650 °C
 243 J
@Temperature -29.0 °C
 273 J
@Temperature 540 °C
 297 J
@Temperature 260 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000886 ohm-cmRT
 0.0000950 ohm-cm
@Temperature 1000 °C
 0.0001011 ohm-cm
@Temperature 900 °C
 0.0001066 ohm-cm
@Temperature 700 °C
 0.0001078 ohm-cm
@Temperature 800 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.3 µm/m-°C
@Temperature 25.0 - 100 °C
 12.9 µm/m-°C
@Temperature 25.0 - 200 °C
 13.6 µm/m-°C
@Temperature 25.0 - 300 °C
 14.3 µm/m-°C
@Temperature 25.0 - 500 °C
 14.3 µm/m-°C
@Temperature 25.0 - 400 °C
 14.6 µm/m-°C
@Temperature 25.0 - 600 °C
 15.1 µm/m-°C
@Temperature 25.0 - 700 °C
 15.8 µm/m-°C
@Temperature 25.0 - 800 °C
 16.5 µm/m-°C
@Temperature 25.0 - 900 °C
 17.0 µm/m-°C
@Temperature 25.0 - 1000 °C
Thermal Conductivity 9.40 W/m-KRT
 10.9 W/m-K
@Temperature 100 °C
 12.9 W/m-K
@Temperature 200 °C
 14.8 W/m-K
@Temperature 300 °C
 16.8 W/m-K
@Temperature 400 °C
 18.7 W/m-K
@Temperature 500 °C
 20.7 W/m-K
@Temperature 600 °C
 22.6 W/m-K
@Temperature 700 °C
 24.7 W/m-K
@Temperature 800 °C
 26.7 W/m-K
@Temperature 900 °C
 29.2 W/m-K
@Temperature 1000 °C
Melting Point 1330 - 1410 °C
Solidus 1330 °C
Liquidus 1410 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.10 %
Chromium, Cr 20 %
Cobalt, Co 51 %
Iron, Fe <= 3.0 %
Manganese, Mn 1.5 %
Nickel, Ni 10 %
Silicon, Si <= 0.40 %
Tungsten, W 15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® L-605 Cobalt-Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal
Haynes 25 alloy, cold worked sheet, 20% cold reduction
ATI Allvac® 35N Nickel Superalloy BIllet, Heat Treatment: 1052°C (1925°F) + Age
Haynes 25 alloy, hot rolled and 1230°C solution annealed sheet
ATI Allvac® Nickelvac® TJA-1537™ UNS R31537 & UNS R31538 Nickel Superalloy, Warm Worked

NH25AT / 16573

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.