Market Segment: Caps and Closures Suggested Uses Include Housewares, Caps and Closures, Fast-Cycle Injection Molding Information provided by Sunoco Chemicals. Available in Canada. Braskem acquired Sunoco Chemicals polypropylene product line in 2010. |
Good Mold Release, Nucleated, Excellent Rigidity and Hardness |