MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Necowel FLE 55N Clay Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: NECOWEL FLE 55N is a zero VOC emulsified alkyd copolymer based on linseed/marine oils.

Applications: Wood Impregnation; Wood Finish. Due to excellent wetting properties and penetration properties, NECOWEL FLE 55N is an excellent binder for water based wood preservatives, sealers and wood stains. According to the type of application, NECOWEL FLE 55N can be diluted with water to a solids content of 10 – 35%. There is no need for the addition of driers, as the product already has the appropriate driers incorporated. The incorporation of a biocide is recommended for the final formula. Wood preservatives, sealers and wood stains based on NECOWEL FLE 55N exhibit adhesion and penetration properties and outstanding weather resistance, which are comparable or better than those of solvent based systems. In combination with acrylates, NECOWEL FLE 55N improves adhesion, weather resistance and reduces thermoplasticity.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 53 - 57 %
pH 6.5 - 7.5
Viscosity 3000 - 4000 cP
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Opibent® 1008 Layered Silicate
BYK Nanothix® B1490 Phylosilicate
BYK Mineral Colloid® MO Clay Additive
BYK Mineral Colloid® BP Bentonite
BYK Laponite® XLS Synthetic Layered Silicate

PBYK075 / 185072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.