MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC 120W Linear Low Density Polyethylene for Blown Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and optical properties.
Formulation: 1500 ppm Slip & 3000 ppm Antiblock

Typical Applications: Ice & frozen food bags, liners, produce bags, bread bags, textile & garment packaging, etc.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccload density; ASTM D1505
Thickness 30.0 microns
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 10.0 MPaASTM D882
Film Tensile Strength at Yield, TD 9.00 MPaASTM D882
Film Elongation at Break, MD 650 %ASTM D882
Film Elongation at Break, TD 810 %ASTM D882
Elmendorf Tear Strength MD 160 gASTM D1922
Elmendorf Tear Strength TD 350 gASTM D1922
Elmendorf Tear Strength, MD 5.33 g/micronASTM D1922
Elmendorf Tear Strength, TD 11.67 g/micronASTM D1922
Dart Drop Total Energy 600 J/cmPuncture Resistance; SABIC Method
Dart Drop 4.00 g/micronASTM D1709
Dart Drop Test 120 gASTM D1709
Film Tensile Strength at Break, MD 38.0 MPaASTM D882
Film Tensile Strength at Break, TD 30.0 MPaASTM D882
1% Secant Modulus, MD 260 MPaASTM D882
1% Secant Modulus, TD 270 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 100 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 10 %ASTM D1003
Gloss 90 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 195 - 215 °C
Blow-up Ratio (BUR) 2.0 - 3.0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® C40 01 PA66/6 (Dry)
SABIC 6821N Linear Low Density Polyethylene for Blown Film
BASF Ultramid® C40LX 01 PA66/6 (Dry)
BASF Ultramid® B40LN 01 PA6 (Dry)
NOVA Chemicals Novapol® PF-Y821-BP Butene LLDPE Film Resin

PSABICZ827 / 133023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.