MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel

Material Notes: Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W and V, gives an extremely high compressive strength, 69 HRC, combined with a very good abrasive wear resistance. For cutting tool applications Uddeholm Vanadis 60 offers a unique combination of high wear resistance, hot hardness and good toughness compared to all other HSS. The P/M process ensures a good machinability and grindability together with a good dimensional stability during heat treatment.

Vanadis 60 is characterized by:

  • High wear resistance
  • Maximum compressive strength
  • Good through hardening properties
  • Good toughness
  • Good dimensional stability on heat treatment
  • Very good temper resistance
Applications: Uddeholm Vanadis 60 is a high alloyed high performance PM high speed steel with an addition of cobalt. Uddeholm Vanadis 60 is particularly suitable for cold work tooling where highest wear resistance and highest compressive strength are required at the same time.

Key Words: W.-Nr. 1.3241
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.286 lb/in³soft annealed
 0.281 lb/in³
@Temperature 600.0 °C
soft annealed
 0.283 lb/in³
@Temperature 399 °C
soft annealed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 340Soft annealed
Hardness, Rockwell C 62 - 69austenitizing 1760-2156°F, temper 3 x 1hr at 1040°F
Modulus of Elasticity 36000 ksi(hardened and tempered)
 20000 ksi
@Temperature 600.0 °C
hardened and tempered
 32000 ksi
@Temperature 399 °C
hardened and tempered
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.90 µin/in-°F
@Temperature 399 °C
hardened and tempered
 6.10 µin/in-°F
@Temperature 600.0 °C
hardened and tempered
Specific Heat Capacity 0.100 BTU/lb-°F
@Temperature 20.0 °C
hardened and tempered
 0.120 BTU/lb-°F
@Temperature 399 °C
hardened and tempered
 0.140 BTU/lb-°F
@Temperature 600.0 °C
hardened and tempered
Thermal Conductivity 21.0 W/m-K
@Temperature 20.0 °C
hardened and tempered
 24.0 W/m-K
@Temperature 600.0 °C
hardened and tempered
 25.0 W/m-K
@Temperature 399 °C
hardened and tempered
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.3 %
Chromium, Cr 4.2 %
Cobalt, Co 10.5 %
Iron, Fe 63 %As Balance
Molybdenum, Mo 7.0 %
Tungsten, W 6.5 %
Vanadium, V 6.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
316 Stainless Steel, annealed sheet
304 Stainless Steel
AISI 4340 Steel, annealed, 25 mm round

NBUCOR17 / 15486

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.