MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Asahi Kasei Stylac™ 20 ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes:

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmASTM D955
Melt Flow 6.0 g/10 min
@Load 9.99 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100
@Thickness 2.50 mm
Tensile Strength, Yield 44.0 MPa50mm/min; ISO 527-1
Flexural Strength 66.0 MPa2mm/min; ISO 178
Flexural Modulus 2150 MPa2mm/min; ISO 178
Charpy Impact, Notched 38.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 60.0 °CRelative Thermal Index; UL 746A
Hot Ball Pressure Test 95.0 °CRegistered Number: B-1560; EMAC
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75-1,2
Vicat Softening Point 101 °C
@Load 5.10 kg
ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accucomp ABS ABS802L High Impact Grade
Aclo Accucomp ABS ABS801L Medium Impact Grade
Ineos ABS Lustran® 448
Ineos ABS Lustran® 648
Aclo Accucomp ABS ABS892BL High Heat Grade

PASAHI8264 / 221288

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.