MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics and resilience. Elastocon® 2825 can be overmolded onto polypropylene.

Information provided by Elastocon® TPE Technologies. Elastocon® TPE Technologies has been acquired by Aurora Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.022 - 0.032 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25ASTM D2240
Tensile Strength, Yield 716 psiASTM D412
Elongation at Break 530 %ASTM D412
100% Modulus 0.105 ksi
@Strain 100 %
ASTM D412
Compression Set 13 %
@Time 79200 sec
ASTM D395B
 
Processing PropertiesOriginal ValueComments
Feed Temperature 175 °F
Rear Barrel Temperature 280 - 320 °F
Front Barrel Temperature 330 - 360 °F
Nozzle Temperature 370 - 400 °F
Mold Temperature 60.0 - 120 °F
Back Pressure 50.0 - 100 psi
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Injection RateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer
AlphaGary Evoprene™ Super G 946 SEBS Thermoplastic Elastomer
A. Schulman DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)
AlphaGary Evoprene™ G 925 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer

PELASC02 / 81646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.