MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec 848 Zirconia, ZrO2•MgO
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Tetragonal zirconia exhibits high flexural strength and superior low temperature stability. It features higher impact strength and erosive wear resistance as compared to alumina. 848 TTZP (yellow) is recommended for applications where high fracture toughness is required, with higher elastic modulus.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.00 g/ccDIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %DIN EN 623-2 / ASTM-C373
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1150HV 0.5; DINV ENV 843-4
Tensile Strength at Break 551 MPaACMA Test #4 / DIN EN 843-1
Tensile Modulus 186 GPaYoung's; DINV ENV 843-2 / ASTM-F417
Flexural Strength 750 MPa20 x 40 mm
Compressive Strength 3000 MPaASTM C-773-88 / DIN 51067T1
Poissons Ratio 0.33DINV ENV 843-2
Fracture Toughness 10.0 MPa-m½DIN 51109
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+13 ohm-cm
@Temperature 500 °C
Dielectric Constant 28
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.60 µm/m-°C
@Temperature 20.0 - 200 °C
 7.70 µm/m-°C
@Temperature 20.0 - 600 °C
ASTM-C373
 8.20 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.400 J/g-°C
@Temperature 100 - 200 °C
DINV ENV 821-3
Thermal Conductivity 2.70 W/m-KDIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 900 °C
 
Descriptive Properties
ColorYellow
Thermal Shock Resistance R1 (K)304Hasselman (Experimental)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec ZN 40 Zirconia, ZrO2-MgO
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
CeramTec MZ 429 Zirconia, ZrO2-Y2O3
Cordierite, 2MgO-2Al2O3-5SiO2

CCERA939 / 107539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.