MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Maxxam® FR PP 301-30 Flame Retardant Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Data provided by PolyOne.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ASTM D792
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 29.0 MPa
@Thickness 3.17 mm
4210 psi
@Thickness 0.125 in
2"/min speed; ASTM D638
Elongation at Break 250 %
@Thickness 3.17 mm
250 %
@Thickness 0.125 in
2"/min speed; ASTM D638
Flexural Modulus 1.24 GPa
@Thickness 3.17 mm
180 ksi
@Thickness 0.125 in
0.2"/min speed; ASTM D790
Izod Impact, Notched 0.370 J/cm
@Thickness 3.17 mm
0.693 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FUL746C
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
@Thickness 3.17 mm
180 °F
@Thickness 0.125 in
ASTM D648
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 V-0
@Thickness 4.00 mm
V-0
@Thickness 0.157 in
VTM
Oxygen Index 28 %28 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fainplast Compounds GK 0185/R Flexible PVC, Flame Retardant Sheathing Lead Free
Cossa Polimeri ESTAPROP K 0200 V2 Flame Retardant Polypropylene
Cheng Yu Plastic PP225 Flame Retardant Polypropylene, Medium Impact
Avient Maxxam® FR PP FR 7B01 Flame Retardant Polypropylene
Avient Maxxam® FR PP FR 7A02 Flame Retardant Polypropylene

PHH468 / 47094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.