MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AdvanSix Aegis® H8202NLB Extrusion Grade Nylon 6
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Product Description: Aegis® H8202NLB is an unfilled, low/medium viscosity, non-lubricated nylon 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It exhibits good strength, stiffness, and toughness as well as excellent heat, chemical and abrasion resistance.

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Water Absorption 1.6 %1.6 %24 hr; ASTM D570
Moisture Absorption <= 0.10 %<= 0.10 %ASTM D6869
Moisture Absorption at Equilibrium 2.7 %2.7 %50% RH; ASTM D570
Water Absorption at Saturation 9.5 %9.5 %ASTM D570
Viscosity Measurement 2.612.6196% SAV
 46 - 5246 - 52FAV; ASTM D789
Linear Mold Shrinkage, Flow 0.0128 cm/cm0.0128 in/inASTM D955
Melt Flow 9.8 g/10 min
@Load 1.00 kg,
Temperature 235 °C
9.8 g/10 min
@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 280 °C464 - 536 °F
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi
 
Descriptive Properties
Extractable Content<0.8%SOP-702-307

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8202C HS BK-102 PA6 (Conditioned)
NYCOA 2047 Copolymer Nylon 6/69
Overview of materials for Nylon 6, Unreinforced
NYCOA 400 PA 6
NYCOA 2062 Copolymer Nylon 6/66

PHONWL166 / 179711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.