MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Rigid Extrusion 87727-0284 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: The Cell Classification was determined using the notched Izod test with injection molded samples. Physical property testing was based on the Geon® 87727 Trans 0020.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 858515 sec; ASTM D2240
Tensile Strength, Yield 56.9 MPa8250 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.87 GPa416 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 93.5 MPa13600 psiASTM D790
Flexural Modulus 2.92 GPa424 ksiASTM D790
Izod Impact, Notched  0.160 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.300 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
 0.350 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.656 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
 2.10 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
3.93 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Dart Drop Total Energy  66.3 J/cm
@Temperature 23.0 °C
0.124 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 175 J/cm
@Temperature 23.0 °C
0.328 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C38.9 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 61.1 °C
@Thickness 3.18 mm
142 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
TP; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Descriptive Properties
AppearanceTranslucent
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification11553ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesCapstock
 Profiles
 Vertical Blinds

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS PCA-2008 Flame Retardant PC/ABS Alloy
Overview of materials for PVC, Extruded
Geon® Performance Solutions Vinyl Rigid Extrusion L6181 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 87020 Exterior Extrusion PVC
Arkema Nakan® RPX 301 L PVC, Rigid Extrusion Grade

PH0POL0521 / 145090

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.