MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil HD 6601.29 High Density Polyethylene (HDPE), Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: HD 6601 is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications offering excellent ESCR with good stiffness-toughness balance.  Ideally suited for articles requiring rugged physical performance in cold temperature environments. 

Availability:  Latin America, North America. 

Additive:  Long term UV-15 stabilizer: yes. 

Applications:  automotive components, industrial components, waste carts, industrial closures, recreational vehicle-components.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.948 g/ccASTM D1505
ESCR 10% Igepal® 20 hourF50; ASTM D1693B
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3400 psiASTM D638
Elongation at Break 1000 %ExxonMobil Method
Flexural Modulus 140000 psi2% secant; ASTM D790B
Flexural Modulus, 1% Secant 160000 psiASTM D790B
Izod Impact, Notched 1.00 ft-lb/in
@Temperature -40.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 266 °FPeak; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 156 °Funannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 108 °Funannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
ExxonMobil HD 6608.19 High Density Polyethylene (HDPE), Injection Molding Grade
Borealis BorPURE™ MB6561 High Density Polyethylene for Injection Molding
Amco PRIMATOP HDPE 055952 Injection Molding Polyethylene
Chevron Phillips LX8119 HDPE Injection Molding Resin

PEX98880 / 238262

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.