MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound DFP34 Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DFP34 compound is based on Polycarbonate (PC) resin containing 20% glass fiber, 15% PTFE/silicone. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccASTM D792
 1.42 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.100 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0036 cm/cm24hrs; ISO 294
 0.0030 - 0.0050 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm24hrs; ASTM D955
 0.0044 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 103 MPaASTM D638
 104 MPaISO 527
Tensile Strength, Yield 103 MPaASTM D638
 103 MPaISO 527
Elongation at Break 2.5 %ISO 527
 2.8 %ASTM D638
Elongation at Yield 2.5 %ISO 527
 2.8 %ASTM D638
Tensile Modulus 6200 MPa1 mm/min; ISO 527
 6890 MPa5 mm/min; ASTM D638
Flexural Strength 158 MPaASTM D790
 158 MPaISO 178
Flexural Modulus 6200 MPaASTM D790
 6400 MPaISO 178
Izod Impact Notched 138 JASTM D256
Izod Impact, Unnotched 720 J/mASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 44.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 24.0 Jpeak; ASTM D3763
Impact Test 6.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.51ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.53ASTM D3702 Modified: Manual
K (wear) Factor 108 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 33.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 36.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 46.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 47.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 145 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 143 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 141 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 V-1
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 310 - 320 °C
Zone 3 320 - 330 °C
Melt Temperature 305 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80723 / 288670

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.