MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® D4270 J (O/E SBS) Branched Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D4270 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene in the neat polymer of 32% mass. It is supplied from Japan in the physical forms identified in the grade nomenclature:
D4270 JSP - supplied as dusted pellets
D4270 JS - supplied as dusted crumb

Region: Japan

Uses: Kraton D4270 J is used for formulating compounds for footwear and general purpose applications and as a modifier of bitumen.

Applications: Bitumen Modification and Compounding and Personal Hygiene

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/cc
Volatiles <= 1.0 %
@Temperature 110 °C,
Time 7200 sec
Melt Flow 10 - 24 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Ash <= 1.0 %ISO 247
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 46
@Time 30.0 sec
ISO 7619
Tensile Strength 12.0 MPaISO 37
Elongation at Break 1100 %ISO 37
300% Modulus 0.00190 GPa
@Strain 300 %
ISO 37
 
Descriptive Properties
ContentBound Styrene32 percent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1155 E (SBS) Liner Block Copolymer
INEOS Styrolution K-Resin® KR03 Styrene Butadiene Copolymer (SBC)
INEOS Styrolution K-Resin® KR01 Styrene Butadiene Copolymer (SBC)
A. Schulman Diamond SBS 1031 Clear Styrene Butadiene Copolymer
Kraton® D1155 B (SBS) Liner Block Copolymer

PKRA9848 / 132747

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.