MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 5216 Epoxy - Unidirectional S-Glass Prepreg, After Environmental Exposure
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM® 5216 is a 200 – 250°F (93 – 121°C) curing, modified epoxy resin. Service temperature range is -67 to 180°F (-55 to 82°C). This prepreg is manufactured by hot melt processing and is virtually solvent-free. Glass fiber reinforced CYCOM 5216 is used in military and commercial helicopter blades and structures and is extensively used for engine nacelles.

Features & Benefits:

  • Available in carbon, aramid and glass fiber prepreg
  • Excellent fatigue resistance
  • High flow with long shop life
  • Autoclave and press cure
  • Maximum continuous service temperature up to 180°F (82°C)
  • Low pressure moldable
  • Good tack and drape characteristics
  • Excellent translation of fiber strength
  • Tape laying machine capable
Applications:
  • Aircraft secondary structure
  • Rotorcraft structure and blade applications
Property data for Standard Cure, S-Glass Fiber, Unidirectional with 52.7% fiber volume. Oil soak = seven days at 160°F (66°C) in MIL-H-83282. Water boil = boiled two hours in distilled water. Temperature exposure = 1000 hours at 180°F (82°C)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.235 g/ccCured, Neat Resin
Volatiles <= 0.30 %
@Time 900 sec
QC-PT-16
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 144000 psi
@Temperature 82.0 °C
0° Orientation, After Oil Soak; ASTM D790
 152000 psi
@Temperature 82.0 °C
0°, After Water Boil; ASTM D790
 165000 psi
@Temperature 23.0 °C
0°, After Water Boil; ASTM D790
 175000 psi
@Temperature 82.0 °C
0° Orientation, After Temperature Exposure; ASTM D790
 180000 psi
@Temperature 23.0 °C
0° Orientation, After Oil Soak; ASTM D790
 199000 psi
@Temperature 23.0 °C
0° Orientation, After Temperature Exposure; ASTM D790
 221000 psi
@Temperature -54.0 °C
0° Orientation, After Temperature Exposure; ASTM D790
 235000 psi
@Temperature -54.0 °C
0°, After Water Boil; ASTM D790
 261000 psi
@Temperature -54.0 °C
0° Orientation, After Oil Soak; ASTM D790
Flexural Modulus 42.0 GPa
@Temperature 23.0 °C
0°, After Water Boil; ASTM D790
 43.0 GPa
@Temperature 82.0 °C
0° Orientation, After Oil Soak; ASTM D790
 43.0 GPa
@Temperature -54.0 °C
0° Orientation, After Oil Soak; ASTM D790
 44.0 GPa
@Temperature -54.0 °C
0°, After Water Boil; ASTM D790
 48.0 GPa
@Temperature 82.0 °C
0°, After Water Boil; ASTM D790
 49.0 GPa
@Temperature 23.0 °C
0° Orientation, After Oil Soak; ASTM D790
 51.0 GPa
@Temperature 23.0 °C
0° Orientation, After Temperature Exposure; ASTM D790
 53.0 GPa
@Temperature -54.0 °C
0° Orientation, After Temperature Exposure; ASTM D790
 54.0 GPa
@Temperature 82.0 °C
0° Orientation, After Temperature Exposure; ASTM D790
Shear Strength 7500 psi
@Temperature 82.0 °C
0° Orientation Short Beam, After Oil Soak; ASTM D2344
 7600 psi
@Temperature 82.0 °C
0° Orientation Short Beam, After Water Boil; ASTM D2344
 10400 psi
@Temperature 23.0 °C
0° Orientation Short Beam, After Water Boil; ASTM D2344
 10700 psi
@Temperature 82.0 °C
0° Orientation Short Beam, After Temperature Exposure; ASTM D2344
 11100 psi
@Temperature 23.0 °C
0° Orientation Short Beam, After Oil Soak; ASTM D2344
 12400 psi
@Temperature 23.0 °C
0° Orientation Short Beam, After Temperature Exposure; ASTM D2344
 13700 psi
@Temperature -54.0 °C
0° Orientation Short Beam, After Oil Soak; ASTM D2344
 15600 psi
@Temperature -54.0 °C
0° Orientation Short Beam, After Temperature Exposure; ASTM D2344
 15700 psi
@Temperature -54.0 °C
0° Orientation Short Beam, After Water Boil; ASTM D2344
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °F
Minimum Service Temperature, Air -67.0 °F
Glass Transition Temp, Tg 88.0 °CWet
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 250 °FCure Temp.
Gel Time 4.00 - 6.00 min
@Temperature 135 °C
Neat Resin
Shelf Life >= 1.00 Month
@Temperature 22.0 °C
 3.00 Month
@Temperature 4.00 °C
sealed container
 6.00 Month
@Temperature -18.0 °C
sealed container

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 5216 Epoxy - Unidirectional S-Glass Prepreg
Solvay CYCOM® 5216 Epoxy - Unidirectional E-Glass Prepreg
Solvay CYCOM® 5216 Epoxy - Unidirectional E-Glass Prepreg, After Environmental Exposure
Solvay CYCOM® 934 Epoxy - E-Glass Fiber Reinforced Unidirectional Tape and Roving Laminate
Solvay CYCOM® 381 Epoxy Prepreg with CYCOM 7781 OST E-glass Fabric and 300FAW Epoxy

PCYTED097b / 193480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.