MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Teflon® PTFE 7C Granular Molding Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Teflon® PTFE white granular molding powders are ideal for molding many different end products and stock shapes. Excellent chemical resistance, electrical properties, high temperature performance, low temperature toughness, plus unique adhesion and flame resistance.

Teflon® PTFE granular molding powders are processed by compressing them into a desired shape and heating them at temperatures above their melting point to consolidate the powder.

Resin Characteristics: Small, fibrous particles with a low bulk density Uses: Usually mixed with inorganic powders to make filled molding compounds that offer improved wear and cold flow resistance.

Typical properties for Teflon® PTFE Granular Resin:

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Polytetrafluoroethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.16 g/ccASTM D4894
Bulk Density 0.250 g/ccASTM D4894
Water Absorption <= 0.010 %24 hours; ASTM D570
Particle Size 28 µmASTM D4894
Linear Mold Shrinkage 0.060 cm/cmat preform pressure of 35 Mpa; ASTM D4894
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 58ASTM D785
Hardness, Shore A 98ASTM D2240
Hardness, Shore D 50 - 65ASTM D2240
Tensile Strength, Ultimate 37.9 MPaASTM D4894
Elongation at Break 400 %ASTM D4894
Flexural Modulus 0.496 GPaASTM D790
Poissons Ratio 0.46approaches a limit of 0.50 at higher temperature
Izod Impact, Notched 189 J/mASTM D256
Coefficient of Friction 0.050 - 0.10ASTM D 1894
Coefficient of Friction, Dynamic 0.10V = 10 fpm; P= 800 - 1000 psi
 0.13V = 100 fpm; P= 80 - 100 psi
Coefficient of Friction, Static 0.050 - 0.080500 psi
K (wear) Factor 2500 x 10-10 in³-min/ft-lb-hrunlubricated vs. soft carbon steel
Limiting Pressure Velocity 1200 psi-ft/min
@Temperature 21.0 - 27.0 °C
at 10 fpm
 1800 psi-ft/min
@Temperature 21.0 - 27.0 °C
at 100 fpm
 2500 psi-ft/min
@Temperature 21.0 - 27.0 °C
at 1000 fpm
Taber Abrasion, mg/1000 Cycles 8.91000 cycles; CS-17F wheel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+18 ohmASTM D257
Dielectric Constant 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm100 micrometers film; ASTM D149
Dissipation Factor <= 0.00010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 300 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 112 µm/m-°C
@Temperature -100 - 25.0 °C
 124 µm/m-°C
@Temperature 25.0 - 100 °C
 220 µm/m-°C
@Temperature 25.0 - 300 °C
 790 µm/m-°C
@Temperature 20.0 - 25.0 °C
Large volume change in the 18-25°C transition range
Specific Heat Capacity 1.20 J/g-°C
@Temperature 40.0 °C
 1.30 J/g-°C
@Temperature 150 °C
 1.40 J/g-°C
@Temperature 20.0 °C
 1.50 J/g-°C
@Temperature 260 °C
Thermal Conductivity 0.250 W/m-K
 0.300 W/m-K
@Temperature 20.0 - 260 °C
Melting Point 317 - 337 °CASTM D4894
Maximum Service Temperature, Air 260 °Cretains useful mechanical properties
Minimum Service Temperature, Air -268 °Cretains useful mechanical properties
 -79.0 °Cremains highly flexible
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 379 - 429 °CCure Temperature
 
Descriptive Properties
20% Hydrochloric Acid Transmission, g/100sq in.<0.01
50% Sodium Hydroxide Transmission, g/100sq in.<.01
Acetic Acid Transmission, g/100sq in.0.41
Acetone Transmission, g/100sq in.0.95
Acetophenone Transmission, g/100sq in.0.5
Benzene Transmission, g/100sq in.0.64
Carbon Tetrachloride Transmission, g/100sq in.0.31
Chemical/Solvent ResistanceExcellent
Detergent Resist. on grit-blasted aluminum, Hours624
Detergent Resistance on aluminum, Hours264
Detergent Resistance on grit-blasted steel, Hours24
Ethyl Acetate Transmission, g/100sq in.0.76
Folding Endurance, # cycles, .18-.20 mm>10^6
Heat of Combustion J/g5100ASTM D240
Hexane Transmission, g/100sq in.0.56
Piperidine Transmission, g/100sq in.0.04
Red Fuming Nitric Acid Transmission, g/100sq in.7.5-1.4
Salt Spray Resistance on aluminum, Hours>744
Salt Spray Resistance on steel, Hours192
Sulfuric Acid Transmission, g/100sq in.0.00001
Water Transmission, g/100sq in.0.4
Weather Resistance20Years unaffected in Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE 7A Granular Molding Powder
Chemours Teflon® PTFE Grade 7B Granular Compression Molding Resin
Chemours Teflon® PTFE 8 Granular Molding Powder
Chemours Teflon® PTFE 850A Granular Molding Powder
Overview of materials for Polyetheretherketone, Unreinforced

PDU901 / 33299

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.