MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 985 Epoxy + Carbon Uni-Tape Laminate
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® 985 is a 350°F (177°C) curing epoxy resin system. CYCOM 985 is designed for use where a balance of performance and processing characteristics is required. It has excellent structural performance and good impact resistance. CYCOM 985 is co-curable with structural adhesives and will produce outstanding thin-skinned sandwich structures. CYCOM 985 allows thick section construction without exotherm problems. Optimum properties are achieved by curing under autoclave pressure from 45 to 100 psi (as appropriate to panel configuration) at 350°F (177°C) for two hours. CYCOM 985 prepregs have good tack and drape and an out-time of two weeks at room temperature.

Features & Benefits:

  • Modified epoxy system
  • Excellent hot/wet strength retention
  • 350°F (177°C) cure
  • Good impact resistance
  • 300°F (149°C) service temperature
  • Controlled flow
  • Ease of processing
  • Good tack and drape
  • 14 day shop life
  • Shelf life of 6 months at 0°F (-18°C)
Applications: Primary and secondary aircraft structures

Mechanical property data for 985 epoxy with 8 ply laminate with 56% fiber volume Carbon Uni-Tape 145 gsm

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 287200 psi
 4900 psi
@Temperature 132 °C
90°, 20 ply
 5300 psi
@Temperature 71.0 °C
90°, 20 ply
 5800 psi
@Temperature 24.0 °C
90°, 20 ply
 6100 psi
@Temperature -54.0 °C
90°, 20 ply
Tensile Modulus 6.20 GPa
@Temperature 132 °C
90°, 20 ply
 6.90 GPa
@Temperature 71.0 °C
90°, 20 ply
 8.30 GPa
@Temperature 24.0 °C
90°, 20 ply
 9.70 GPa
@Temperature -54.0 °C
90°, 20 ply
 121 GPa
@Temperature -54.0 °C
 128 GPa
@Temperature 24.0 °C
 129 GPa
@Temperature 71.0 °C
 133 GPa
@Temperature 132 °C
Compressive Strength 1172 MPa
@Temperature 71.0 °C
 1207 MPa
@Temperature 24.0 °C
Wet
 1241 MPa
@Temperature 24.0 °C
 1275 MPa
@Temperature -54.0 °C
Compressive Modulus 121000 MPa
@Temperature 132 °C
 123000 MPa
@Temperature 71.0 °C
 124000 MPa
@Temperature -54.0 °C
 124000 MPa
@Temperature 24.0 °C
Shear Strength 6300 psi
@Temperature 132 °C
Short Beam, wet
 8800 psi
@Temperature 132 °C
Short Beam
 9000 psi
@Temperature 71.0 °C
Short Beam, wet
 10900 psi
@Temperature 24.0 °C
Short Beam, wet
 11500 psi
@Temperature 71.0 °C
Short Beam
 17000 psi
@Temperature 24.0 °C
Short Beam
 17400 psi
@Temperature -54.0 °C
Short Beam
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 149 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 350 °F
@Time 7200 sec
Cure
Shelf Life 6.00 Month
@Temperature -17.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 5320-1 Epoxy with T40/800B Unidirectional Tape Composite
Solvay CYCOM® 890 RTM Resin - Woven Carbon Fabric Composite
Solvay CYCOM® 977-3 Epoxy - Unidirectional Carbon Fiber Tape
Solvay CYCOM® 5250-4 RTM BMI Resin, Composite with IM7-6K-4HS Fabric
Solvay CYCOM® 5250-4 RTM BMI Resin, Composite with T650-35-3K-PW Fabric

PCYTED092b / 234740

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.