MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, Mill-Hardened UNS C17410, 1/2 HT
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Applications: strip and wire: fuse clips, fasteners, springs, diaphragms, lead frames, switch parts, and electrical connectors; rod and plate: resistance spot welding tips, die casting plunger tips, and tooling for plastic molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 95Strip
Tensile Strength, Ultimate 725 MPaStrip
Tensile Strength, Yield 620 MPaStrip
Elongation at Break 15 %In 50 mm, Strip
Modulus of Elasticity 138 GPa
Machinability 25 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000382 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 233 W/m-K
Melting Point 1025 - 1065 °C
Solidus 1025 °C
Liquidus 1065 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 450 - 550 °CHeat-treating temperature
Hot-Working Temperature 650 - 925 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.20 %
Beryllium, Be 0.15 - 0.50 %
Cobalt, Co 0.35 - 0.60 %
Copper, Cu 99.2 %
Iron, Fe <= 0.20 %
Silicon, Si <= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Brass
Eagle Brass 101 OFE COPPER (Certified), 1/2 Hard
Beryllium Copper, UNS C17200, TD02 Temper Strip
Beryllium Copper, UNS C17200, TH02 Temper Strip
Beryllium Copper, UNS C17000

MC17410b1 / 10892

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.