MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: BorSafe™ ME3420 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an optimized stabilization system. BorSafe™ ME3420 is classified as an MRS 8.0 material (PE80). Applications: BorSafe™ ME3420 is recommended for pressure pipe systems in the applications field of: drinking water, natural gas, industrial, relining, geothermal collector, and irrigation particularly where flexibility and coil ability is of importance. Thanks to its bimodal structure, it also shows excellent resistance to rapid crack propagation and slow crack growth.

Information provided by Borealis AG

Key Words: PE;MDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.948 g/ccISO 1183
Environmental Stress Crack Resistance >= 5.0 hour
@Pressure 0.800 MPa,
Temperature 80.0 °C
ISO 13479
Oxidative Induction Time (OIT) >= 20 min
@Temperature 200 °C
EN 728
Melt Flow 0.40 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 19.0 MPa50mm/min; ISO 527-2
Elongation at Break >= 600 %ISO 527-2
Flexural Modulus 700 MPaISO 178
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 180 - 210 °Ccylinder
Die Temperature 200 - 210 °C
Melt Temperature 200 - 220 °C
Head Temperature 200 - 210 °C
 
Descriptive Properties
Resistance To Rapid Crack Propagation (bar)7S4 test, Pc at 0°C, test pipe 250mm, SDR11, ISO 13477

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem GM5340PR High Density Polyethylene
Braskem HF0144 High Density Polyethylene
Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation
Carmel Olefins Ipethene® 100 Low Density Polyethylene
Carmel Olefins Ipethene® 4203 Low Density Polyethylene

PBOREA354 / 108614

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.